r/electroplating • • 8h ago

Chromate peeling off

Thumbnail gallery
3 Upvotes

Hello, I work at a shop that does silver and zinc plating.

Our zinc process is: prep pieces (jangle it, sandblast, wire-wheel finish), dip in an acid + distilled water bath, 20 min plating, acid dip, chromate (15 sec), distilled water rinse, compressed air, dry.

I'll upload photos of our setup, chemicals, and peel-off

It looks like it's only the chromate layer peeling off, not the actual zinc plating.

I've worked here for under a year and did zinc plating for a few months.

Acid + distilled water bath ratio is around 5% acid, 95% water (I made a mistake by eyeballing the ratio)

We thought the chromate was weak, so we added more chromate, but it still peels off.

I think we tried all possible ways I can think of.

But you guys are smarter than me, so help, thanks!