Hello all,
I am attempting to recreate this paper for production of aqueous stable ZnONPs from Zn(acetate)2 and O2 @ 900 C. I am struggling with a few things, as this is my first attempt at sol-gel preparation of nanoparticles. First, I assumed that it would be necessary to remove the solvent (in this case H2O) prior to firing. I've tried both with and without drying, and I believe I got better results from not drying (but other factors could have also contributed). It may have been due to not utilizing less oxygen while wet, I am unsure. Also, maybe I am not leaving enough solvent prior to pouring the gel.
The first trial (wet) resulted in very clean looking ZnO, but only a small portion was actually soluble in the 5% trisodium citrate solution, I even tried sonicating the crap out of it. It appeared to consist primarily of macroparticles. Also, I believe I had the oxygen flowrate too low because when the crucibles were placed into the tube furnace flames began shooting out of the tube furnace, and when I turned the oxygen up to see what happened the flames disappeared and only gas/soot appeared to be leaving the tube furnace after. The majority of the product was lost in this rapid expansion during combustion.
The second trial was boiled down much thicker and was left to dry in a drying oven overnight prior to firing. During firing the oxygen flow rate was much higher (although the dial accidentally got turned to low in adjusting to try to find the optimal rate, which again resulted in rapid expansion and flames, albeit much less and for a much shorter duration than trail 1. The oxygen flowrate was rapidly increased as immediately upon turning the dial a loud almost explosive expansion occured). Much less product was lost this time, but despite being left for longer than the cited ~15 min firing in the paper (perhaps 20-25 min), the product was full of soot that was essentially impossible to seperate following the methods in the paper (MeOH wash). It was able to be separated in the MeOH based on the density, but the soot was essentially insoluble.
Anyway, any appreciation or advice from anyone with more knowledge of the sol-gel process than myself is greatly appreciated. Specifically I am wondering what the "optimal amount of water" they don't bother to quantify in the paper is, and how thick I should make the sol before pouring. I am kind of thinking as soon as the slurry is formed, that it should be poured and then dried in the drying oven then left with an excess of oxygen @ 900 c until i can pull the quartz tube out and see no more soot left in the crucible.
Thanks, I really appreciate it!
EDIT: I am also wondering about surface area in the crucible, as my crucibles are more round to fit in my tube furnace